SEM photos of Aluminum corrosion with KI electrolyte : March 7 2009

squidbaby 2.jpg

squidbaby 3.jpg

squidbaby 4 25000x.jpg

pixie 12 squidhole2 tendrils01.jpg

Pixie 12 outer surf 36 hr 25000x.jpg

Pixie 12 outer surf 48 hours squid form01.jpg

Pixie 12 squid form 48 hours 750x 30kv 01.jpg

Pixie 12 squid form 48 hours 750x 30kv 02.jpg

pixie 12 outer 72 hour squidhole02.jpg

Pixie 12 outer surf 72hr 160x 60 deg 01.jpg

Pixie 12 outer surf 72hr 1000x 60 deg 01.jpg

pixie 12 outer 72 hour squid01.jpg

pixie 12 outer 72 hour squid02.jpg

pixie 12 outer 72 hour squidhole01.jpg